LOCTITE ECCOBOND EO1062

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND EO1062

Main features

  • Low flow
  • Non conductive
  • Excellent reliability

Product Description

LOCTITE ECCOBOND EO 1062 is designed to pass 1,000 hours of temperature/humidity/bias testing and thermal cycling up to 125°C. Exceptional viscosity stability at 25°C provides easier control of shot size using conventional time/pressure dispensing equipment.

 

Cure Schedule

  • 4 to 6 hours @ 125°C - Robust non-stress sensitive components
  • 3 hours @ 140°C.  - Stress sensitive components 
Product Family

EO1062/30C0

30cc Syringe - 397695
1. Select Package Type
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 50 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Unit of measure Syringe
Net weight 51 g
Gross weight 67 g
Dimensions 2.2 x 2.2 x 11.8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
600 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.78
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
125 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.90000000000000 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
64,000 mPa.s

Leading Brands Trust in Our Products and Services